MG Midget and Sprite Technical - Minor Body Filling

Do you remember, fifty-oddd years ago, how we filled little chips and dips with a one-part filler - in a tube I think.
I need about 1cc of filler, and don't want to mix a great lump of two-part.

Perhaps I am imagining this.
Nick and Cherry Scoop

Nick, I have used a 1K knifing filler from HB for very small jobs, I think it was 980, but I didn't get on very well with it.

It might be due to my poor skills but despite several applications and careful sanding back with very fine grit paper I could never make the repair disappear completely.

Whatever you decide to use, I recommend doing some test pieces before committing it to the car.

Colin
C Mee

You can get 'stopper' in 2 part and cellulose which is intended for filling very minor defects. I've always found it sands easier than filler.
David Billington

In my experience:
One part knifing filler/ stopper is ok for small blemishes when flatting primer but 1cc is fairly substantial (a dint?) and is probably best filled with 2 part filler. Depends on depth. A pain if that's all you need but it lasts a while (for the next dint....). I'm interested in other opinions though.
Bill B

Something like this Nick? Or it may be too fine for your needs?

https://www.amazon.co.uk/MP-Essential-Bodywork-Scratches-Detailing/dp/B08YFHH4JN/ref=sr_1_4?sr=8-4

Jeremy MkIII

Thank you for these suggestions.
I expect I'm exaggerating when I say 1cc. It's for a number of areas where we've knocked paint off during our recent ten days away. We jumped in and out a lot, and obviously managed to knock the doors out of fit. So the flange of the A-post got scraped by the door shutting, and the other door went the opposite way - abrasive contact between the rear end of the alloy capping and the top of the B-post. Plus a couple of other tiny chips.

We're not precious about perfect paintwork, but I don't want a lot of naff-looking touch-ups.
Nick and Cherry Scoop

All the air dried stoppers and fillers will shrink, so you need a few coats. It's annoying that they usually come in enormous tubes or tins such as in Jeremy's photo. Holts knifing putty comes in a much smaller tube but isn't very good - too stiff and poor adhesion. I still use it though, just in thin layers. Crucial of course to clean out pits and chips and get any suggestion of polish out. For a very small stone chip I sometimes put a tiny blob of undiluted cellulose in it. This often needs 2-3 coats, until it's slightly proud, then when hard I flat down after applying a skin of filler. Once flatted with a block you know the blob has gone when the filler has gone. Then of course you have to polish. Works well on cellulose.
Les Rose

I have been using this stuff. Holts cataloy knifing stopper. Slow to harden but works well and sands off nicely. 100g tube so you would have enough, but not too much!

GuyW

Thanks Les; thanks Guy. I reckon that Holts putty would do it. We'll see how it survives on vulnerable edges.
Then I just need to find a small quantity of RD4.
Nick and Cherry Scoop

I typed that before reading Les' comment saying it doesnt stick well! I haven't found a problem so long as the substrate is very clean and of course, dry.

But as Les says, for paint chips I just build up several applications of paint with a very small artist's brush. But I like the idea of topping it off with a contrasting filler before sanding back.
GuyW

I think the main issue with the Holts product is that it's a bit too stiff. It's better if you make sure that the hardened skin that forms under the cap is discarded so that you get softer material. However, I don't usually use it on panel edges, where something tougher such as 2K filler is better. For door edge chips I just apply thick cellulose and flat and polish when hard.
Les Rose

Its a bit like colemans mustard, you throw away more than you use each time. Colemans were said to make their profit on what was left on your plate at the end of your meal.

GuyW

I'm sharing a tube with my pal who's doing up a Sunbeam Alpine. Maybe if we get together, we can pass the knife back and forth. One in the eye for Colemans.
Nick and Cherry Scoop

Just one question. How many hours/days do you allow for Holt's Cataloy putty to dry before sanding?
Nick and Cherry Scoop

It goes on very thinly, Nick. It's really intended for very shallow surface dints and imperfections. Applied thinly, I find it hardens ok. I put it on and then leave it until the next day before sanding. If I sand too soon I will find it has skinned over ok but not set underneath.
GuyW

Thanks Guy. I'll give it a day or so.
Nick and Cherry Scoop

I confess I have never painted anything, and I need some advice.
How do you get the shine back, after rubbing down/T-cutting etc? The two-pack paint is so bloody shiny.
Nick and Cherry Scoop

Nick
In my experience: Rub down with 400/500 paper, then 1000 and possibly 1500. You should now have a matt looking finish. Then use t-cut or, better, Farecla G3 rubbing compound with a bit of water then buff with a clean microfibre cloth and the shine will return. This works well on celly but will also work on 2 pack.

Some people (especially pro's) use an electric polisher but it's easy to "burn through" the paint (or laquer with 2 pack) if you're not careful, especially celly.
Bill B

Nick, the door has been rubbed down or "flatted" probably with up to 1000 paper while the bonnet has also been compounded with G3. This was celly which went on with a rather rough texture as it was sprayed outside and was drying too quickly as it hit the metal.

Bill B

Didn't turn out too bad although celly dulls over time and you have to cut and polish again which is why people prefer 2 pack. Celly is easier to touch in though.

Bill B

Looks nice Bill. Shiny, but not harsh like some 2 pack finishes.
GuyW

Really useful, Bill. Thank you.
I need some finer paper - off to get that now.
Lovely job on your car; how did you get the bonnet to sit in so beautifully behind the wheel?
Nick and Cherry Scoop

Nick
I think it was a combination of sufficient adjustment and luck! The short inside struts at the rear outer part of the bonnet that fasten to both the bonnet top and wing upper are adjustable and pull the rear of wing inwards.. Also I found that pulling the lower front of the wings forward slightly resulted in tbe lower wings behind the wheel also pulling inward. I then found this was due to the upper wing above the top of the wheelarch being weak so I reinforced this area on the inside.
Bill B

Nice work, Bill. I remember, years ago, Guy suggested that the stiffening plates just forward of the adjusting struts might be carefully twisted to pull the wings in. A bit like your strengthening measures.
Nick and Cherry Scoop

Yes, it must have been those stiffening plates I had to re-inforce due to corrosion. Anyway, it's still ok! The Frogeye front end is a large hunk of metal isn't it and can be challenging to align.
Bill B